type: dislotungsten
references:
- D. Cereceda et al.,
International Journal of Plasticity 78:242-265, 2016,
http://dx.doi.org/10.1016/j.ijplas.2015.09.002
- A. Koester et al.,
Acta Materialia 60:3894-3901, 2012
http://dx.doi.org/10.1016/j.actamat.2012.03.053
output: [Lambda_sl]
N_sl: [12]
b_sl: [2.72e-10]
rho_mob_0: [1.0e+9] # estimated from section 3.2
rho_dip_0: [1.0] # not given
Q_s: [2.61154e-19] # 1.63 eV, Delta_H0
B: [8.3e-5]
omega: [9.1e+11] # nu_0
p_sl: [0.86]
q_sl: [1.69]
tau_Peierls: [2.03e+9]
h: [2.566e-10]
h_sl-sl: [0.009, 0.72, 0.009, 0.05, 0.05, 0.06, 0.09]
w: [2.992e-09] # 11b
i_sl: [1] # c, eq. (25)
D: 1.0e+20 # d_g, eq. (25)
D_a: 1.0 # d_edge = D_a*b
# values in Cereceda et al. are high, using parameters from Koester et al.
a_nonSchmid: [0.61, 0.23, 0.55] # Table 1
D_0: 0.0 # disable climb
f_at: 1