DAMASK_EICMD/examples/Marc/material.yaml

32 lines
690 B
YAML

---
homogenization:
SX:
N_constituents: 1
mechanical: {type: pass}
phase:
Aluminum:
lattice: cF
mechanical:
output: [F, P, F_e, F_p, L_p, O]
elastic: {type: Hooke, C_11: 106.75e9, C_12: 60.41e9, C_44: 28.34e9}
plastic:
type: phenopowerlaw
N_sl: [12]
a_sl: 2.25
atol_xi: 1.0
dot_gamma_0_sl: 0.001
h_0_sl_sl: 75e6
h_sl_sl: [1, 1, 1.4, 1.4, 1.4, 1.4]
n_sl: 20
output: [xi_sl]
xi_0_sl: [31e6]
xi_inf_sl: [63e6]
material:
- homogenization: SX
constituents:
- phase: Aluminum
v: 1.0
O: [0.9330127018922194, 0.25, 0.06698729810778066, 0.25]