diff --git a/examples/config/phase/mechanical/plastic/dislotungsten_W.yaml b/examples/config/phase/mechanical/plastic/dislotungsten_W.yaml index 6a0e4dcc2..6efe77644 100644 --- a/examples/config/phase/mechanical/plastic/dislotungsten_W.yaml +++ b/examples/config/phase/mechanical/plastic/dislotungsten_W.yaml @@ -3,6 +3,10 @@ references: - D. Cereceda et al., International Journal of Plasticity 78:242-265, 2016, http://dx.doi.org/10.1016/j.ijplas.2015.09.002 + - A. Koester et al., + Acta Materialia 60:3894-3901, 2012 + http://dx.doi.org/10.1016/j.actamat.2012.03.053 +output: [Lambda_sl] N_sl: [12] b_sl: [2.72e-10] rho_mob_0: [1.0e+9] # estimated from section 3.2 @@ -12,18 +16,19 @@ B: [8.3e-5] omega: [9.1e+11] # nu_0 p_sl: [0.86] q_sl: [1.69] -tau_Peierls: [2.03e+9] # there is also tau_c^* = 2.92GPa, not clear in the paper +tau_Peierls: [2.03e+9] h: [2.566e-10] -a_nonSchmid: [0.938, 0.71, 4.43] h_sl-sl: [0.009, 0.72, 0.009, 0.05, 0.05, 0.06, 0.09] w: [2.992e-09] # 11b i_sl: [1] # c, eq. (25) D: 1.0e+20 # d_g, eq. (25) D_a: 1.0 # d_edge = D_a*b +# values in Cereceda et al. are high, using parameters from Koester et al. +a_nonSchmid: [0.61, 0.23, 0.55] # Table 1 + D_0: 0.0 # disable climb f_at: 1 Q_cl: 1.0 -output: [Lambda_sl] v_0: [1]