diff --git a/examples/config/Phase_DisloUCLA_Tungsten.config b/examples/config/Phase_DisloUCLA_Tungsten.config index e680213d5..1eef32577 100644 --- a/examples/config/Phase_DisloUCLA_Tungsten.config +++ b/examples/config/Phase_DisloUCLA_Tungsten.config @@ -6,21 +6,8 @@ plasticity disloucla (output) dipole_density (output) shear_rate_slip (output) accumulated_shear_slip -(output) mfp_slip (output) resolved_stress_slip (output) threshold_stress_slip -(output) twin_fraction -(output) shear_rate_twin -(output) accumulated_shear_twin -(output) mfp_twin -(output) resolved_stress_twin -(output) threshold_stress_twin - -### Material parameters ### -lattice_structure bcc -C11 523.0e9 # From Marinica et al. Journal of Physics: Condensed Matter(2013) -C12 202.0e9 -C44 161.0e9 grainsize 2.7e-5 # Average grain size [m] 2.0e-5 SolidSolutionStrength 0.0 # Strength due to elements in solid solution