DAMASK_EICMD/examples/config/phase/mechanical/plastic/phenopowerlaw_Pt-5%Cu.yaml

20 lines
386 B
YAML
Raw Normal View History

2022-05-13 14:40:02 +05:30
type: phenopowerlaw
2022-05-17 02:46:23 +05:30
2022-05-13 14:40:02 +05:30
references:
2022-05-17 02:46:23 +05:30
- K.M. Jackson and C. Lang,
Platinum Metals Review 50:15-19, 2006,
https://doi.org/10.1595/147106705X93359,
fitted to Fig. 5 (Pt-5% Cu recrystallised)
output: [xi_sl, gamma_sl]
2022-05-13 14:40:02 +05:30
N_sl: [12]
n_sl: 20
a_sl: 0.9
h_0_sl-sl: 781.2e+6
xi_0_sl: [114.e+6]
xi_inf_sl: [207.e+6]
h_sl-sl: [1, 1, 5.123, 0.574, 1.123, 1.123, 1]
dot_gamma_0_sl: 0.001