DAMASK_EICMD/examples/config/phase/mechanical/plastic/phenopowerlaw_Au.yaml

25 lines
583 B
YAML
Raw Normal View History

type: phenopowerlaw
2022-02-12 23:11:59 +05:30
2021-05-24 13:32:28 +05:30
references:
- D. Ma et al.,
2021-07-14 00:16:50 +05:30
Acta Materialia 103:796-808, 2016,
https://doi.org/10.1016/j.actamat.2015.11.016
2021-05-24 13:32:28 +05:30
- I. Kovács and G.Vörös,
2021-07-14 00:16:50 +05:30
International Journal of Plasticity 12:35-43, 1996,
https://doi.org/10.1016/S0749-6419(95)00043-7
2021-08-14 16:31:37 +05:30
- U.F. Kocks,
Metallurgical and Materials Transactions B 1:11211143, 1970,
https://doi.org/10.1007/BF02900224
2022-02-12 23:11:59 +05:30
2021-05-24 13:32:28 +05:30
output: [xi_sl, gamma_sl]
2022-02-12 23:11:59 +05:30
N_sl: [12]
2022-02-12 23:11:59 +05:30
2021-05-24 13:32:28 +05:30
n_sl: 83.3
a_sl: 1.0
h_0_sl-sl: 75.0e+6
2021-06-29 14:52:42 +05:30
xi_0_sl: [26.25e+6]
xi_inf_sl: [53.0e+6]
2021-06-25 18:55:35 +05:30
h_sl-sl: [1, 1, 1.4, 1.4, 1.4, 1.4, 1.4]
dot_gamma_0_sl: 0.001